Muab ternary thermoelectric bismuth telluride P-hom Bi0.5Sb1.5Te3 thiab N-hom Bi2Te2.7Se0.3
Kev taw qhia luv luv
Khoom npe:P-hom Bi0.5Sb1.5Te3
N-hom Bi2Te2.7Se0.3
Purity: 99.99%, 99.999%
Appearance: Thaiv ingot los yog hmoov
Hom Tshuaj: Epoch-Chem
Muab ternary thermoelectric bismuth tellurideP-hom Bi0.5Sb1.5Te3thiabN-hom Bi2Te2.7Se0.3
Kev ua tau zoo
Lub TIG-BiTe-P / N-2 thermoelectric ingot yog zus nrog cov alloy ntawm Bi, Sb, Te, Se, tshwj xeeb doping thiab peb cov txheej txheem crystallizing tshwj xeeb.Lub Bi2Te3-raws li thermoelectric ingot yog zus tshwj xeeb thiab optimized rau ua cov thermoelectric modules uas siv los hloov cov cua sov qhov chaw xws li 100 ℃ (373K) mus rau 350 ℃ (623K) rau hauv hluav taws xob.Feem ntau, qhov nruab nrab ntawm qhov zoo ZT ntawm peb cov p-hom thiab n-hom ingots tshaj qhov kub ntawm 300K txog 600K yog loj dua 0.7.Lub module ua nrog xws li ingots tuaj yeem ua tiav 5% kev ua haujlwm nrog 250 ℃ Delta T. Meanwhile, peb ingot yog featured nrog zoo mechanical zog thiab ruaj khov khoom, muab lub pob zeb tseem ceeb rau kev ua tau zoo thiab txhim khu kev qha fais fab modules.
Yam khoom | bismuth telluride, bi2te3 |
N hom | |
P hom | Bi0.5Te3.0Sb1.5 |
Specification | Thaiv ingot los yog hmoov |
ZT | 1.15 |
Ntim | vacumm hnab ntim khoom |
Daim ntawv thov | tub yees, cua txias, thermo, kev tshawb nrhiav kev tshawb fawb |
Hom | Epoch |
Daim ntawv thov
Los tsim P / N hlws ris, siv nyob rau hauv semiconductor tub yees, thermoelectric hmoov tiam thiab lwm yam.
Specification
Specificaiton | P-hom | N-hom | Sau tseg |
Ntaus tus lej | Peb-P-2 | BiTe N-2 | |
Txoj kab uas hla (mm) | 31 ± 2 | 31 ± 2 | |
Ntev (mm) | 250 ± 30 | 250 ± 30 | |
Qhov ceev (g / cm3) | 6.8 | 7.8 ib | |
Hluav taws xob conductivity | 2000-6000 | 2000-6000 | 300 K |
Seebeck Coefficient α (μ UK-1) | ≥140 | ≥140 | 300 K |
Thermal conductivity k (Wm-1 K) | 2.0-2.5 hli | 2.0-2.5 hli | 300 K |
Hmoov Factor P (WmK-2) | ≥0.005 | ≥0.005 | 300 K |
ZT nqi | ≥0.7 | ≥0.7 | 300 K |
Hom | Epoch-Chem |